Mfr Part #: ASTA-7G#Made with 99.8% pure micronized silver.#62% to 65% silver content by weight.#Superior thermal conductivity. Greater than 7.5 W/mK#Temperature range: - 40C to 150C (Bond strength is weakened at temperatures below 0C due to crystallization.)#Negligible electrical conductivity.#